In recent years there has been greater awareness of the
harmful effects of lead, and there have been efforts around the world
to curb the use of this metal. Matsuo Handa was quick to recognize this
problem and set about developing a lead-free solder. There are still many
problems that need to be resolved regarding restrictions on the use of
lead and the changeover to lead-free products. |
@ |
![]() |
FLF Series |
|||||
|
Alloy No.
|
Alloy Composition
|
Melting Temperature
|
Flux Core (with resin)
|
Bar
|
Paste
|
|
FLF
01 |
Sn-3.0Ag-0.5Cu
|
217-218
|
|||
|
FLF
02 |
Sn-3.5Ag
|
221
|
|||
|
FLF
03 |
Sn-0.7Cu
|
228
|
|||
Tensile Strength Test JIS II Testing Sample |
![]() |
|
Test conducted by the Kanagawa Industrial Technology
Testing Center
|
@